• Bauxite 40% limes to no 40%, 15% iron oxide.
• As Since CA is not present, suitable to sea and under-water work.
• It’s rapid hardening properties arises due to Al2O3.CaO. For setting and hardening 
there is not free hydrated lime as in the case of OPC.
• Final setting 600 minutes.
• One day strength is 30N/mm2 and 3 day is 35N/mm2
.
• Not be used in places where temperature exceeds 180C.
• Fineness ≥ 225 m2
/Kg.
• Expansion ≤ 5mm.
• Used widely for pre-casting.

Sulphate Resisting Portland Cement (SRPC) (IS: 12330)

• It contains very low C3A.
• Expansion of cement is limited to 10 mm and 0.8 per cent, when tested by Le-
chatelier method and autoclave test, respectively.
• Setting times are same as that for ordinary Portland cement.
• Fineness of 400 m2/kg.
• Initial setting time ≤ 30 minutes and final setting time ≥ 600 minutes.
• Strongly recommended for structures in sea water.